product name:Metal ceramic structural adhesive

origin:

application:Model: Licheng LC8613
Appearance: Milky white semi liquid
Proportion: 1:1
Packaging specification: 10kg/set
Storage period: 12 months

sales hotline:+86-0354-3965688

Usage: Used for bonding wear-resistant materials such as corundum lining, alumina lining, microcrystalline stone slab, and cast stone slab with metal bodies. This product has high adhesive strength, fast curing speed, and stable adhesion on the facade and top without flowing.



Product parameter table:


 

Parameter

Specifications

Number of times

detection result 

Temperature resistance (℃)

4*4*0.5

5 times average value

180℃

Compression shear bonding strength

AB/Metal

5 times average value

22.3MPa

Tensile shear strength

AB/Metal

5 times average value

15.29

Operating time(min)

AB mixture

5 times average value

30min

Curing Time(min)

AB mixture

5 times average value

12h

Test conditions: temperature 23 ± 2 ℃, relative humidity 50 ± 5%.

Note: When the temperature is below 10 ℃, appropriate heating measures should be taken, otherwise the curing time will be prolonged. When the temperature is below 0 ℃, place it in a room with a temperature not lower than 20 ℃ for 5-8 hours before use, or place it in hot water not higher than 50 ℃ to release the colloidal crystallization state before use. If conditions permit, it can also be placed on a radiator to remove colloidal crystallization. The placement time depends on the ambient temperature, approximately 0.6-3 hours.